A New Copper Age? Copper Alloy Rivals Superalloy Strength
Researchers developed a Cu-Ta-Li alloy with thermal stability and strength comparable to superalloys while retaining copper’s conductivity, ideal for high-temperature use.
Researchers developed a Cu-Ta-Li alloy with thermal stability and strength comparable to superalloys while retaining copper’s conductivity, ideal for high-temperature use.